YLTPACK News Industry News Causes and solutions of sticky layout after flexographic plate making

Causes and solutions of sticky layout after flexographic plate making

Table of Contents

Reasons for the sticky layout after flexographic plate making: 1. The plate is not cleaned after being washed and corroded. 2. The rinse solution has been used for too long or the active ingredients are insufficient. Solution: 1. After the plate is washed and corroded, it is thoroughly cleaned. 2. Replace the flushing solvent. For more information, our customer service. ! !