YLTPACK › Blog › Heat Sealable Plastic Bags: PE vs CPP, Settings and Leaks

Heat Sealable Plastic Bags: PE vs CPP, Settings and Leaks

Laminated heat sealable plastic bags beside a bar sealer showing a clean top seal
Heat Sealable Plastic Bags: PE vs CPP, Settings and Leaks
Summarize this article with:ChatGPTClaudePerplexityGeminiGrok

Which sealant layer makes a bag heat sealable: PE or CPP?

Heat sealable plastic bags seal because their inner sealant layer melts and fuses at a lower temperature than the outer films. That layer is usually PE (polyethylene) or CPP (cast polypropylene). PE suits most dry food, frozen and liquid packs. CPP and its retort grade RCPP are the choice when the pack must survive hot-fill or 121 °C sterilisation.

A sealant layer is the inner film of a laminate that melts under the jaws and bonds to itself. A laminate structure is the stack of films bonded together, listed outer layer first, such as PET/VMPET/PE.

Cross-section of PET/VMPET/PE pouch film showing the PE sealant layer melting under heat seal jaws

The outer layer carries the print and does none of the sealing. It’s usually PET (polyester), a stiff film that takes heat well, or BOPP (biaxially oriented polypropylene), a cheaper film with a lower heat limit.

Sealant thickness drives hot-tack, which is how well a seal holds while it’s still warm. That matters on a form-fill-seal line, where product drops onto a bottom seal closed a fraction of a second earlier.

Metallocene PE (mPE) is a PE grade that seals at lower heat with high hot-tack and can seal through light powder dust. CPP is a polypropylene sealant film with good clarity and heat resistance. The figures below are typical values from resin and film datasheets.

Sealant Starts sealing at Typical thickness Use it for
LDPE/LLDPE 105–125 °C 50–150 μm Most dry and frozen food
mPE 90–110 °C 50–100 μm Powders, fast VFFS lines
CPP 130–150 °C 30–70 μm Hot-fill, clear snack bags
RCPP 140–160 °C 50–100 μm 121 °C retort meals, wet pet food

LDPE/LLDPE covers most orders. We suggest mPE only when the product is dusty or the line runs fast, and a PP sealant only when the fill is hot.

Don’t trim the sealant to save money. Going from 60 μm to 80 μm adds a little to the unit price, while one pallet of leaking pouches costs you the product plus the reshipment.

A mono-PE pouch is a laminate made entirely of polyethylene, usually BOPE (biaxially oriented PE) outside and PE inside, so it can go into PE recycling streams. The EU Packaging and Packaging Waste Regulation (PPWR) is pushing brands this way as its recyclability rules phase in.

Mono-PE seals close to LDPE temperatures at 40–100 μm, but its window is only about 10–15 °C wide. The outer layer can also stick to hot jaws, and the pouch stands less stiffly. PTFE-coated jaws or PTFE tape stop the sticking. If your sealer holds temperature tightly, the switch is realistic after a trial.

Do impulse sealers and band sealers need different films?

Yes, impulse sealers and band sealers need different film features. An impulse sealer suits plain PE and thin PET/PE laminates but struggles with thick nylon or foil laminates. A band sealer needs a heat-resistant outer layer such as PET. BOPP or mono-PE outers need lower heat or PTFE-coated bands.

Heat sealable plastic bags pe vs cpp settings and 2 1200x630

As a typical working limit, a standard single-element impulse sealer seals PE and PET/PE reliably up to about 100 μm per wall. Above that, or with foil or nylon in the structure, the short heat pulse doesn’t reach the sealant, so use a constant-heat sealer, a band sealer or a double-sided impulse model. On band sealers, a BOPP outer starts to shrink not far above 150 °C and a BOPE outer softens earlier, so run those cooler and slower.

A VFFS (vertical form fill seal) machine forms bags from roll stock film around a tube, fills them from above and seals them in one cycle. An HFFS (horizontal form fill seal) machine does the same with the film running flat. A premade pouch machine opens, fills and seals pouches that arrive already made.

Run a 250 g ground coffee bag in PET/AL/PE through a band sealer at full speed and the seals come out weak and cloudy, because the foil pulls heat away. Slowing the band or adding 10 °C fixes it. A 1 kg frozen-vegetable bag in plain PE seals fine on an impulse sealer, yet a 140 μm PET/NY/PE laminate in the same sealer peels open by hand.

Dwell time is how long the jaws stay closed on the film. It typically runs 0.5–2 s plus cooling on impulse sealers, 0.5–1.5 s on constant-heat bars, often under 0.5 s on VFFS and HFFS jaws, and 0.5–1.0 s on premade pouch machines. Band sealers set dwell by belt speed.

Tell your supplier the sealer model and jaw type. Serrated and flat jaws need different settings for the same laminate.

What temperature, pressure and dwell time should you use?

Start heat sealable plastic bags in PET/PE on a constant-heat bar at 150–180 °C, 0.2–0.3 MPa (about 30–45 psi) and 0.5–1.0 s dwell, then fine-tune with a seal curve. Mono-PE runs cooler, around 120–140 °C. Foil and retort structures need more heat and a longer dwell. Your film and your jaws decide the final numbers.

Temperature, pressure and dwell work together, so change one at a time. We can give you a starting window. Your own machine confirms it.

Get the structure right before you touch the dial. PET/PE is enough for dry snacks. Coffee needs PET/AL/PE for oxygen and light barrier, liquids need NY/PE for puncture resistance, and retort needs PET/RCPP.

Then size the sealant and seal width to the fill weight. A 100 g stand-up pouch (about 120 x 180 mm + 70 mm gusset) needs 50–60 μm sealant and an 8 mm seal. A 500 g zipper pouch (160 x 230 mm + 80 mm) needs 70–80 μm and 10 mm, and a 1 kg flat bottom bag (140 x 320 mm, 90 mm side gusset) needs 80–100 μm and 10 mm.

At 2.27 kg / 5 lb (240 x 350 mm, 120 mm gusset), go to 100–120 μm and 12 mm. A 6.8 kg / 15 lb side gusset handle bag (330 x 560 mm, 140 mm gusset) needs 120–150 μm and 12–15 mm. A 500 ml spout pouch (160 x 260 x 45 mm) typically uses 100 μm NY/PE with a 10 mm seal. These sizes are suggested starting points, confirmed against your fill weight, density and filling line, usually with a fill test on samples.

The settings below assume a 10 mm flat constant-heat bar and are confirmed on 15 mm test strips sealed in 10 °C steps.

Structure Temperature Pressure Dwell
PET/PE 150–180 °C 0.2–0.3 MPa 0.5–1.0 s
MOPP/PET/PE 140–170 °C (BOPP outer limits heat) 0.2–0.3 MPa 0.5–1.0 s
PET/AL/PE 160–190 °C 0.2–0.3 MPa 0.8–1.5 s (foil draws heat away)
NY/PE 150–180 °C 0.2–0.3 MPa 0.5–1.0 s
Mono-PE 120–140 °C 0.2–0.3 MPa 0.5–1.0 s
PET/RCPP 180–210 °C 0.3–0.4 MPa 1–2 s

Band sealers run a step hotter, so adjust belt speed before you add heat. Impulse sealers usually have fixed pressure: start low on the heat dial and always allow full cooling.

Find the temperature where the seal stops peeling, and the one where the edge turns glassy or the outer film puckers. Run in the middle of that gap, not at the top of it.

A funnel or dust guard plus 30–40 mm of headspace above the fill keeps product off the seal. Write the settings down per SKU and per sealer, so the night shift doesn’t guess. On 5,000 pouches, a 2% leak rate means 100 bags lost with their product, plus a reship and possibly a retailer complaint.

Why do heat seals leak, wrinkle or peel?

Heat seals usually fail for one of four reasons: product trapped in the seal, wrinkles where the gusset folds cross, settings outside the sealant’s window, or a sealant too thin for the fill. Defective film is a less common cause. The symptom on the failed bag usually tells you which one you’re dealing with.

Take a hand-filled protein powder pouch with channel leaks at the top seal. Fine dust stops the PE from fusing. A funnel or seal guard fixes it, and so does wiping the seal area or switching to an mPE sealant.

Four common heat seal faults on stand-up pouch top seals
Symptom Likely cause Fix
Channel leaks or pinholes at gussets The seal crosses four film layers at the gusset folds More pressure, slightly longer dwell or softer jaw rubber
Wrinkled or puckered seals Temperature too high so the outer layer shrinks, or uneven film feed Lower by 10 °C, check jaw alignment
Seal peels apart easily Cold seal or contamination Raise temperature or dwell, clean the seal area
Bag breaks just beside the seal line Over-sealing has made the film brittle at the edge Lower the temperature
Delamination in the seal area Lamination bond or curing, not your settings Ask the supplier for bond strength results

Settings fix the first four. Delamination goes back to the converter.

Quick checks on a failed bag

Peel it by hand first. If the film tears before the seal opens, the seal fused properly. A clean, shiny peel points to a cold or contaminated seal.

Squeeze the bag under water to find the leak point, usually a gusset corner or a zipper end. If many bags fail at the same jaw position, look at the machine, not the film.

How do I test seal strength before a full production run?

Test heat sealable plastic bags as filled samples closed on your own machine before you approve a full run. The minimum is an ASTM F88 peel test for seal strength plus a bubble or vacuum leak test. Add a drop or compression test for liquids and for fills over about 1 kg.

ASTM F88 is the standard peel test that measures the force needed to pull a seal strip apart. The targets below are typical purchase-spec values, not requirements of the standards. The retort target applies to strips cut after the 121 °C cycle, which weakens seals.

Test What it shows When to ask Typical pass target
ASTM F88 peel Seal strength, N/15 mm Every new structure About 15+ for light snacks, 25+ for heavy fills and liquids, often 40+ for retort
ASTM F2054 burst Weakest point of the whole pouch Liquids, heavy fills Agreed minimum burst pressure
ASTM F2096 bubble leak Gross leaks under internal pressure Powders, coffee, liquids No continuous bubble stream
ASTM D3078 vacuum leak Leaks under vacuum in water Shipping, air freight No bubbles at the set vacuum
Drop test Seal survival in handling Fills over 1 kg, liquids No leaks after the agreed drops

Flat-strip lab results don’t replace a test on your own filled bag, because gussets, zippers and your jaws only show up in the real pack. Ask for both.

Heat sealable plastic bags pe vs cpp settings and featured 1200x630

Run a trial on your own line

  1. Ask for 50–100 samples of the exact structure, enough to test several settings.
  2. Seal strips in 10 °C steps and peel each one to find the window where the film tears before the seal opens.
  3. Fill and seal at least 20 bags at the middle setting, at normal line speed with your real product.
  4. Leak-test them under water or in a vacuum chamber, and drop heavy fills and liquids from the height in your spec.
  5. Send any failed bags back to the supplier with the settings you used.

How we handle seal testing at YLTPACK

YLTPACK recommends the sealant structure and thickness from your product, fill weight and sealer model. Our in-house lab runs air-tightness (leak) and material tensile tests. Before shipping, every finished order passes an 11-point QC inspection that covers seals, air-tightness and lamination.

We have 20+ years in flexible packaging and a 6,520 m² cleanroom workshop with 30+ machines, 11 of them bag-making machines. Free samples come from our stock for your trial (you pay the freight). For a trial with your own artwork, digital printing starts at 1,000 pcs per design, with a lead time of 7–15 days after artwork approval.

Frequently asked questions

How do I seal pouches without a pouch machine?

Use an impulse sealer for plain PE and thin PET/PE pouches. Thick foil or nylon laminates need a band sealer or a constant-heat sealer. Match the sealer’s seal width to the bag size.

Can sealed poly bags be resealed after opening?

No, not by heat on the cut edge. If you need reclosing, specify a press-to-close or slider zipper. You can also leave 20–30 mm of film above the tear notch for a second heat seal.

Do recyclable mono-PE pouches seal as well as PET/PE?

Yes, provided the settings stay inside mono-PE’s narrower window of about 10–15 °C. Run a seal curve trial on samples before you switch a live SKU.

How wide should the seal be?

Most retail pouches need 8–10 mm. Heavy fills and liquids need 10–15 mm. Wider seals also tolerate small wrinkles better.

What seal strength should I ask for?

Ask for about 15 N/15 mm or more on ASTM F88 for light snacks, and 25 N/15 mm or more for heavy fills and liquids. These are typical purchase-spec values, not legal minimums. Agree the number and the test method in writing before the first order.

Can I seal through powder or oil on the seal area?

Sometimes. Metallocene PE sealants tolerate light dust, but oil and heavy powder still cause leaks. Clean filling is the cheaper fix.

The right bag is the one tested on your sealer

The bag to approve is the one that passes peel and leak tests after it has been filled with your product and closed on your own sealer. Specify the sealant by fill weight and sealer type, and set the temperature from a seal curve. A slightly thicker sealant costs less than one batch of returns.

Most failures in heat sealable plastic bags come from a poor match between bag and machine, rarely from the bag alone.

What to send your supplier

Paste this checklist into your first email. Our guide on how custom pouch orders work explains what happens after that.

  • Product: name, fill weight, bulk density, filling method and fill temperature
  • Sealer: type and model, jaw type and current settings
  • Seal spec: required seal strength and test method
  • Barrier: shelf-life target, barrier needs and any recyclability target
  • Samples: enough for a fill-and-seal trial

Request free samples (you pay the freight) and run them through your own sealer with your product. Send us the product, fill weight, sealer model and target quantity through our contact page. We’ll reply within one business day with a suggested structure, starting seal settings and a quote.

Feynman
Written by
Feynman
COO, YLTPACK
20+ YearsSource FactoryCleanroom ProductionFDAISO 9001ISO 22000GRS

Feynman is COO at YLTPACK, a source-factory manufacturer of custom flexible packaging founded in 2005. Drawing on 12 years of hands-on experience in flexible packaging, he oversees production and technical support across the company's 6,520 sqm cleanroom facility and its ISO 9001, ISO 22000 and GRS certified processes, using FDA-compliant food-contact materials. He works directly with global brand owners and procurement teams to turn real sourcing requirements into reliable, compliant pouches.

More about Feynman →LinkedIn

Contact Our Support Team

Contact Us for a Quote. Find the Perfect Solution for Your Project with Us.

100% privacy – We will never spam you!